References
1. Engel, F.K. ¡®Magnetic Tape From the Early Days to the Present' Journal of the Audio Engineering Society 36:7/8 July/August 1988.
2. Carison, D. J. & Milnera, S.M. ¡®Hydrolysis of Resin-Coated Poly(ethylene Terephthalate) Yarns' Journal of Applied Polymer Science 27 (1982).
3. Fox, B. ¡®Tape Life - An Era of Concern' Studio Sound, December 1990.
4. Stosich, M. N. ¡®Archival Revival' Audio, November 1990
5. Brown, D.W., Lowry, R. E., & Smith, L.E. ¡®Prediction of the Long Term Stability of Polyester-Based Recording Media' NBSJR 82-2530 June 1982.
6. Meuller, R. Communication through BASF Australia, April 1991.
7. Curtis, J., ¡®Environmental Aging of Magnetic Tapes' Ampex Corporation, Applied Technology Development: February 1988.
8. Layne, F., Ampex Corporation. ¡®Seminar on Tape Stability and Preservation' NFSA Canberra: August 1991.
9. Cuddihy, E. ¡®Kinetics of the Humid Aging of Magnetic Recording Tape' IEEE Trans. On Magnetics 18:5 September 1982.
10. Ram, T. ¡®Tutorial on the Conservation of Motion Picture Film' NFSA, Canberra: January 1992.